Blog

deep drawing die

Selection of drawing die steel

Drawing dies stretch and deform metal sheets between a punch and a die to produce a cup-shaped workpiece. Their effectiveness depends on excellent wear resistance and anti-seizure properties. In many applications, choosing the right tool steel is critical. For example, steels like D2, D3, H13, H11, 1.2379, 1.2080, 1.2343, or 1.2344 can achieve optimal performance. […]

Selection of drawing die steel Read More »

Classification of Die Steel

Die steel, as a variety of materials to shape the “mother”, is indispensable in industrial production. They are not uniform, but according to the different working environment and needs, finely divided into three categories: Cold work die steel: As the name suggests, this type of steel is mainly used in molds at room temperature or

Classification of Die Steel Read More »